Decode aluminum and PH stainless temper designations like T651, T7351, H32 and H1025 in plain English.
Type a full designation (alloy and temper) or just the temper. The decoder breaks down each letter and digit per the Aluminum Association / ANSI H35.1 temper system, flags combinations that don’t make sense, and explains precipitation-hardening stainless conditions such as Condition A, H900 and H1150.
Enter a designation
Try one:
What it means
For reference only. Mechanical properties and processing limits are set by the governing spec (AMS, ASTM, ANSI H35.1). Confirm against the cert and purchase order.
Aluminum temper designation reference
Basic tempers
| Temper | Meaning |
|---|---|
| F | As fabricated. No control over thermal conditions or strain hardening; no mechanical property limits. |
| O | Annealed. Lowest strength, highest ductility and formability. |
| H | Strain hardened (non-heat-treatable alloys: 1xxx, 3xxx, 5xxx). |
| W | Solution heat-treated. Unstable; the alloy continues to age at room temperature. |
| T | Thermally treated to produce a stable temper other than F, O or H (heat-treatable alloys: 2xxx, 6xxx, 7xxx). |
T tempers
| Temper | Process |
|---|---|
| T1 | Cooled from an elevated-temperature shaping process and naturally aged |
| T2 | Cooled from hot working, cold worked, and naturally aged |
| T3 | Solution heat-treated, cold worked, and naturally aged |
| T4 | Solution heat-treated and naturally aged |
| T5 | Cooled from hot working and artificially aged |
| T6 | Solution heat-treated and artificially aged |
| T7 | Solution heat-treated and overaged/stabilized (T73, T74, T76 trade strength for stress-corrosion or exfoliation resistance) |
| T8 | Solution heat-treated, cold worked, and artificially aged |
| T9 | Solution heat-treated, artificially aged, then cold worked |
| T10 | Cooled from hot working, cold worked, and artificially aged |
Stress-relief suffixes
| Suffix | Meaning | Example |
|---|---|---|
| _51 | Stress relieved by stretching (plate 1.5–3% permanent set; rolled or cold-finished bar 1–3%). No further straightening. | 6061-T651, 7075-T7351 |
| _510 | Extrusions stress relieved by stretching. No further straightening. | 6061-T6510 |
| _511 | Extrusions stress relieved by stretching. Minor straightening allowed to meet tolerances. | 6061-T6511, 2024-T3511 |
| _52 | Stress relieved by compressing (1–5% permanent set). | 7075-T7352 |
| _54 | Stress relieved by combined stretching and compressing (e.g., die forgings restruck cold). | T654 |
H tempers
The first digit after H gives the process: H1 strain hardened only, H2 strain hardened then partially annealed, H3 strain hardened then stabilized, H4 strain hardened then lacquered or painted. The second digit gives the hardness: 2 = quarter hard, 4 = half hard, 6 = three-quarter hard, 8 = full hard, 9 = extra hard. A third digit marks a variation, such as H112 (as worked, with property limits) or H116 (5xxx tested for exfoliation and intergranular corrosion for marine use).
17-4 PH and 15-5 PH conditions
Condition A is solution treated and is usually machined in that state. The part is then aged: the number after H is the aging temperature in °F. H900 gives the highest strength and lowest toughness. H1025 and H1075 balance strength and toughness. H1150 gives the best toughness and stress-corrosion resistance. H1150M is double aged for maximum ductility.
Sourcing a specific temper?
Search Material Harbor for suppliers stocking the alloy and temper you need, from 6061-T651 plate to 17-4 PH bar in Condition A.
Subscribe to the Material Harbor Newsletter
New suppliers and materials on the platform, free engineering tools, and supply chain notes from aerospace engineers. About once a month. No spam, unsubscribe anytime.